AMCO METALS
DUPLEX STEEL- 2205

DUPLEX STEEL- 2205

Send Inquiry
Product Description

DUPLEX STEEL- 2205

Duplex 2205 is a two-phase, ferritic, austenitic 22% chromium, 3% molybdenum, 5 to 6% nickel alloyed stainless steel. It is the most widely used duplex stainless steel grade and is characterized by high yield strength, double that of the standard austenitic stainless steel grades. It also demonstrates good fatigue strength, as well as outstanding resistance to stress corrosion cracking, crevice, pitting, erosion, and general corrosion in severe environments.

Combining many of the beneficial properties of both ferritic and austenitic steels, 2205 is the most widely used duplex stainless steel grade. Its high chromium and molybdenum content gives the stainless steel excellent corrosion resistance. The microstructure provides resistance to stress corrosion cracking and ensures high strength.

The grade is generally not suitable for use at temperatures above 300oC or below -50oC because of reduced toughness outside this range.

You are most likely to encounter 2205 stainless steel being used in industrial environments such as petrochemical, chemical, oil, gas and paper plants.

Alternative Grades

2205 has been available for several years - in general this complies with UNS grade designation S31803. More recently, product has become available complying with the higher corrosion resistant composition UNS S32205, as in table 1. Both these alternatives are known as 2205. 

Chemical Properties:


CMnSiPSCrMoNiN
2205
(S31803)
0.03
max
2.0
max
1.0
max
0.03
max
0.02
max
min: 21.0
max: 23.0
min: 2.5
max: 3.5
min: 4.5
max: 6.5
min: 0.08
max: 0.20
2205
(S32205)
0.03
max
2.0
max
1.0
max
0.03
max
0.02
max
min: 22.0
max: 23.0
min: 3.0
max: 3.5
min: 4.5
max: 6.5
min: 0.14
max: 0.20

Mechanical Properties:

GradeTensile Strength
ksi (min)
Yield Strength
0.2% ksi (min)
Elongation %Hardness (HB) MAX
2205906525217

Physical Properties:


Density
lbm/in3
Electrical
Resistivity
mW•in
Thermal
Conductivity
(BTU/hr•ft•°F)
Heat
Capacity
BTU/lbm•°F
Electrical
Resistivity
(in x 10-6)
at 68°F0.27827.68.70.11233.5
at 212°F
26.19.20.11935.4
at 392°F
25.49.80.12737.4
at 572°F
24.910.40.13439.4